Thiourea Leaching. In order to compare gold dissolution from the ore with and without pretreatment for another lixiviant, the system of thiourea-ferric sulfate was chosen. Figure 9 shows the results for gold leaching at [SC(NH2)2]0 of 0.15 M (11.4 g/L) and [Fe+3]0 of 0.02 M (1.12 g/L) and pH 2.